| NO DIE MARK BENDING | |||
| QViPVjDIE | WING BEND | ||
![]() |
DIE MARK OCCURS AFTER BENDING. | ![]() |
LITTLE DIE MARK OCCURS DUE TO THE GENTLE BENDING |
| THE COVERED VINYL IS TORN AND THE DIE MARK OCCURS AFTER BENDING ALUMINUM AND STAINLESS STEEL. |
![]() |
NO DIE MARK OCCURS FOR BENDING SUCH AS ALUMINUM, STAINLESS STEEL AND THE COVERED MATERIALS. THE COVERED VINYL IS NOT TORN. YOU CAN GET YOUR REQUIRED ANGLE BECAUSE OF NO USAGE OF URETHANE SHEET. |
|
| THE URETHANE SHEET IS PUT ON THE DIE TO PREVENT DIE MARK, BUT YOU HAVE TO CHANGE IT INTO NEW ONE EVERY 10-20 BENDING CYCLE TIMES. THE PRODUCTIVITY GOES DOWN AND IT COSTS HIGH. THE BENDING ANGLE CHANGES EVERY BENDING. |
![]() |
LITTLE DIE MARK OCCURS FOR BENDING SUCH THE PRE-PAINTED MATERIAL. |
|